Tube eccentricity fig. 1

Tube eccentricity fig. 2

Tube eccentricity fig. 3

Tube eccentricity fig. 1

Figure 4
The installation helped improve the tube quality in two ways. First, it reduced the eccentricity’s magnitude; second, it reduced the eccentricity’s variation.